性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
物理性能 | 比重 | ASTMD792 | 1.19 | g/cm³ | |
物理性能 | 吸水率(23°C,24hr,0.250mm) | ASTMD570 | 0.50 | % | |
机械性能 | 耐磨耗性2(23°C) | ASTMD1044 | 23haze | % | |
薄膜 | 薄膜厚度-经测试 | 250 | µm | ||
薄膜 | 膜刺穿强度3(250µm) | ASTMD3763 | 4.60 | J | |
薄膜 | 割线模量 | MD:250µm | ASTMD882 | 1500 | MPa |
薄膜 | 割线模量 | TD:250µm | ASTMD882 | 1400 | MPa |
薄膜 | 抗张强度 | MD:屈服,250µm | ASTMD882 | 41.0 | MPa |
薄膜 | 抗张强度 | TD:屈服,250µm | ASTMD882 | 40.0 | MPa |
薄膜 | 抗张强度 | MD:断裂,250µm | ASTMD882 | 59.0 | MPa |
薄膜 | 抗张强度 | TD:断裂,250µm | ASTMD882 | 52.0 | MPa |
薄膜 | 伸长率 | MD:屈服,250µm | ASTMD882 | 7.0 | % |
薄膜 | 伸长率 | TD:屈服,250µm | ASTMD882 | 7.0 | % |
薄膜 | 伸长率 | MD:断裂,250µm | ASTMD882 | 180 | % |
薄膜 | 伸长率 | TD:断裂 | ASTMD882 | 200 | % |
薄膜 | 落锤冲击4 | -30°C,250µm | ASTMD1709A | 910 | g |
薄膜 | 落锤冲击4 | 23°C,250µm | ASTMD1709A | 880 | g |
薄膜 | 裤型撕裂耐性5 | MD:250µm | ISO6383-1 | 11.0 | N/mm |
薄膜 | 裤型撕裂耐性5 | TD:250µm | ISO6383-1 | 11.0 | N/mm |
薄膜 | 透氧率(23°C,250µm,50%RH) | ASTMD3985 | 32 | cm³·mm/m²/atm/24hr | |
薄膜 | 水气透过率 | 23°C,100%RH,250µm | ASTMF1249 | 4.0 | g/m²/24hr |
薄膜 | 水气透过率 | 38°C,100%RH,250µm | ASTMF1249 | 11 | g/m²/24hr |
薄膜 | CarbonDioxidePermeability6(23°C,254.0µm) | ASTMD1434 | 150 | cm³·mm/m²/atm/24hr | |
薄膜 | ElmendorfTearStrength | MD:23°C,250.0µm | ASTMD1922 | 5 | N |
薄膜 | ElmendorfTearStrength | TD:23°C,250.0µm | 6 | N | |
薄膜 | PPTTearResistance | MD:23°C,250.0µm | ASTMD2582 | 42 | N |
薄膜 | PPTTearResistance | TD:23°C,250.0µm | ASTMD2582 | 56 | N |
薄膜 | 抗撕裂蔓延性7 | MD:23°C,250.0µm | ASTMD1938 | 410 | gf |
薄膜 | 抗撕裂蔓延性7 | TD:23°C,250.0µm | ASTMD1938 | 310 | gf |
薄膜 | 薄膜厚度-经测试 | 250 | µm | ||
薄膜 | 膜刺穿强度3(250µm) | ASTMD3763 | 4.60 | J | |
薄膜 | 割线模量 | MD:250µm | ASTMD882 | 1500 | MPa |
薄膜 | 割线模量 | TD:250µm | ASTMD882 | 1400 | MPa |
薄膜 | 抗张强度 | MD:屈服,250µm | ASTMD882 | 41.0 | MPa |
薄膜 | 抗张强度 | TD:屈服,250µm | ASTMD882 | 40.0 | MPa |
薄膜 | 抗张强度 | MD:断裂,250µm | ASTMD882 | 59.0 | MPa |
薄膜 | 抗张强度 | TD:断裂,250µm | ASTMD882 | 52.0 | MPa |
薄膜 | 伸长率 | MD:屈服,250µm | ASTMD882 | 7.0 | % |
薄膜 | 伸长率 | TD:屈服,250µm | ASTMD882 | 7.0 | % |
薄膜 | 伸长率 | MD:断裂,250µm | ASTMD882 | 180 | % |
薄膜 | 伸长率 | TD:断裂 | ASTMD882 | 200 | % |
薄膜 | 落锤冲击4 | -30°C,250µm | ASTMD1709A | 910 | g |
薄膜 | 落锤冲击4 | 23°C,250µm | ASTMD1709A | 880 | g |
薄膜 | 裤型撕裂耐性5 | MD:250µm | ISO6383-1 | 11.0 | N/mm |
薄膜 | 裤型撕裂耐性5 | TD:250µm | ISO6383-1 | 11.0 | N/mm |
薄膜 | 透氧率(23°C,250µm,50%RH) | ASTMD3985 | 32 | cm³·mm/m²/atm/24hr | |
薄膜 | 水气透过率 | 23°C,100%RH,250µm | ASTMF1249 | 4.0 | g/m²/24hr |
薄膜 | 水气透过率 | 38°C,100%RH,250µm | ASTMF1249 | 11 | g/m²/24hr |
薄膜 | CarbonDioxidePermeability6(23°C,254.0µm) | ASTMD1434 | 150 | cm³·mm/m²/atm/24hr | |
薄膜 | ElmendorfTearStrength | MD:23°C,250.0µm | ASTMD1922 | 5 | N |
薄膜 | ElmendorfTearStrength | TD:23°C,250.0µm | 6 | N | |
薄膜 | PPTTearResistance | MD:23°C,250.0µm | ASTMD2582 | 42 | N |
薄膜 | PPTTearResistance | TD:23°C,250.0µm | ASTMD2582 | 56 | N |
薄膜 | 抗撕裂蔓延性7 | MD:23°C,250.0µm | ASTMD1938 | 410 | gf |
薄膜 | 抗撕裂蔓延性7 | TD:23°C,250.0µm | ASTMD1938 | 310 | gf |
弹性体 | 撕裂强度 | 开裂8 | ASTMD1938 | 12 | kN/m |
弹性体 | 撕裂强度 | 开裂9 | ASTMD1938 | 13 | kN/m |
热性能 | 熔融温度 | 110 | °C | ||
热性能 | 线形热膨胀系数-流动(23°C,0.250mm) | ASTMD696 | 9.0E-5 | cm/cm/°C | |
热性能 | 比热 | 60°C | DSC | 1700 | J/kg/°C |
热性能 | 比热 | 100°C | DSC | 1900 | J/kg/°C |
热性能 | 比热 | 150°C | DSC | 2200 | J/kg/°C |
热性能 | 比热 | 200°C | DSC | 2400 | J/kg/°C |
热性能 | 比热 | 250°C | DSC | 2600 | J/kg/°C |
光学性能 | 光泽度(60°,250µm) | ASTMD2457 | 161 | ||
光学性能 | 折射率 | ASTMD542 | 1.550 | ||
光学性能 | 透射率(250µm) | ASTMD1003 | 92.0 | % | |
光学性能 | 雾度(250µm) | ASTMD1003 | 0.70 | % | |
光学性能 | 黄度指数(250mm) | ASTMD1925 | 0.50 | YI | |
光学性能 | UVTransmittance10(250.0µm) | 89 | % | ||
补充信息 | SurfaceEnergy | Dispersive:23°C,250.0µm | ASTMD5946 | 39 | dyne/cm |
补充信息 | SurfaceEnergy | Polar:23°C,250mm | ASTMD5946 | 8 | dyne/cm |
补充信息 | SurfaceEnergy | Total:23°C,250.0µm | ASTMD5946 | 46 | dyne/cm |